Standards
AWS A5.35 | UWE7014-1A |
---|
Chemical Composition of Weld Metal % (Typical)
C | Si | Mn | Ni |
---|---|---|---|
0.05 | 0.30 | 0.50 | 0.30 |
Mechanical Properties (Typical)
Conditions | Yield Strength (N/mm2) | Tensile Strength (N/mm2) | lmpact Strength IS0-V(J) -20°C | Impact Strength (ISO-V) (Joule) (0°C ) | Elongation ((Lo=5do) (%) |
---|---|---|---|---|---|
Level1 | min. 350 | min. 490 | — | min. 50 | min. 8 |
Wet | 484 | 539 | 44 | 53 | 11 |
Typical Base Material Grades
- Mild Steels, Carbon Steels
Features and Applications
- Designed for general underwater wet welding applications up to 20m water depth.
- Simple to use in all positions in fresh and salt water.
- Provides high quality welding seam in accordance with International Standards in underwater welding applications.
- Modified rutile flux coating offering a continuous weld shape beads.
- Waterproof coating prevent the solubility of the hydrogen from the water to weld metal and provides diver’s safety.
- Good root and sidewall penetration and overhead fusion properties.
- Easy to strike and re-strike.
- Best at filling large gaps and weld metal deposition rate. Easy slag removal.
Current Type
- D.C. (-) or D.C. (+)
Operating Data
Product Code | Welding Current (A) | Weight g / 100 pcs | Diameter x Length (mm) |
---|---|---|---|
3030100099 | 140-180 | 3350 | Ø 3.2 x 350 |
3030100100 | 160-210 | 5000 | Ø 4.0 x 350 |