Пруток и проволока сплошного сечения для сварки теплоустойчивых сталей SG CrMo 2 Si

Standards

TS EN ISO 21952-A

: G CrMo 2 Si

EN ISO 21952-A

: G CrMo 2 Si

TS EN ISO 21952-A

: W CrMo 2 Si

EN ISO 21952-A

: W CrMo 2 Si

AWS A5.28

: ER 90 S-G

Chemical Composition of Welding Wire % (Typical)

C

Si

Mn

Mo

Cr

0.08

0.6

1.0

1.0

2.4

Mechanical Properties

Yield Strength (N/mm2)

Tensile Strength (N/mm2)

Impact Strength (ISO-V/+20°C)

Elongation ((Lo=5do) (%)

Heat Treatment

min. 540

620 — 760

min. 47 J

min. 20

7200C/1hour-3000C air

Typical Base Material Grades

• 10 CrMo9-10, 10 CrSiMoV 7, 10 CrV 63, G-17 CrMo 9-10, A 335 Gr. P22

Features and Applications

• Used for the welding of high heat resisting

•MXoCarlloyed steels which are used for the production of boilers tubes, pipes and nitrided steels

•ldWmetal is resistant to temperatures up to +600°C

• Shielding gases: MAG; Ar+CO2 and Ar+O2 mix gases, TIG; pure Ar gas can be used

Current Type

TIG D.C.(-) / MAG D.C.(+)