Пруток и проволока сплошного сечения для сварки теплоустойчивых сталей SG CrMo 5

Standards

TS EN ISO 21952-A : G / W CrMo 5 Si

EN ISO 21952-A: G / W CrMo 5 Si

AWS A5.28/(A5.9): ER 80 S-B6

Chemical Composition of Welding Wire % (Typical)

C

Si

Mn

Mo

Cr

0.07

0.45

0.5

0.6

6.0

Mechanical Properties

Yield Strength (N/mm2)

Tensile Strength (N/mm2)

Impact Strength (ISO-V/+20°C)

Elongation ((Lo=5do) (%)

Heat Treatment

min. 470

min. 590

min. 70 J

min. 18

730-7600C/1h/3000C air

Typical Base Material Grades

•GX12CrMo5,

Features and Applications

• Used for the welding of high heat resisting steels, hot hydrogen plants, working temperature is +600°C and also used for the welding of steels with 5 Cr 1/2 Mo

• Shielding gases: TIG: pure Ar gas can be used. MAG; Ar+CO2, and Ar+O2 mix gases can be used

Current Type

TIG D.C.(-) / MAG D.C.(+)