Пруток и проволока сплошного сечения для сварки теплоустойчивых сталей SG CrMo 1 Si

Standards

TS EN ISO 21952-A

: G CrMo 1 Si

EN ISO 21952-A

: G CrMo 1 Si

TS EN ISO 21952-A

: W CrMo 1 Si

EN ISO 21952-A

: W CrMo 1 Si

AWSA5.28

: ER 80 S-G

Chemical Composition of Welding Wire % (Typical)

C

Si

Mn

Mo

Cr

0.10

0.6

1.0

0.5

1.2

Mechanical Properties

Yield Strength (N/mm2)

Tensile Strength (N/mm2)

Impact Strength (ISO-V/+20°C)

Elongation ((Lo=5do) (%)

Heat Treatment

min. 470

550 — 670

min. 47 J

min. 20

680°C/1hour-300°C air

Typical Base Material Grades

• 13CrMo4-5, 15CrMo5, 42CrMo4, 16CrMoV4, 25CrMo4, 24CrMo5, G22CrMo5-4, G17CrMo5-5

Features and Applications

• Used for the welding of high heat resisting. Cr-Mo alloyed steels which are used for the production of boilers tubes and pipes and nitrided steels

•ldWmetal is resistant to temperatures up to +570°C

Shielding gases: MAG; Ar+CO2 and Ar+O2 mix gases, TIG; pure Ar gas can be used

Current Type

TIG D.C.(-) / MAG D.C.(+)